Preparing nano-crystalline rare earth doped WC/Co powder by high energy ball milling
Authors:Sha Liu   Ze-Lan Huang   Gang Liu  Gui-Bin Yang
Affiliation:

aSchool of Materials Science and Engineering, Central South University, Changsha, Hunan 410083, PR China

bChongyi Zhangyuan Tungsten Co. Ltd., Chongyi, Jiangxi 341300, PR China

Abstract:The nano-crystalline rare earth doped WC/Co powder was prepared by high energy ball milling. The nano-crystalline powders were characterized by means of XRD (X-ray diffraction), SEM (scanning electron microscope) and DTA (differential thermal analysis). The results show that adding trace rare earth elements into carbides is effective to minish the grain size of WC/Co powder. The grain size of rare earth doped powder became two times smaller as compared with the undoped powder within ball milling times of 25–45 h. The XRD peak of Co phase disappeared after 25 h ball milling. A sharp peak of heat release at the temperature of 597 °C was emerged in DTA curve within the range of heating temperature. After consolidated the rare earth doped WC/Co alloy by high energy ball milling exhibits ultra-fine grain sizes and better mechanical properties.
Keywords:Cemented carbide   Nano-crystalline powder   Rare earth   High energy ball milling
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号