Abstract:The selective HCl leaching method was used to remove phosphorus from high phosphorus iron ores. The hydroxyapatite in high phosphorus iron ores was converted into soluble phosphate during the process of HCl leaching. The effects of reaction time, particle size, hydrochloric acid concentration, reaction temperature, liquid-solid ratio and stirring strength on the dephosphorization ratio were studied. The results showed that the dephosphorization ratio can exceed 98% under the conditions of reaction time 30-45 min, particle size <0. 147 mm, hydrochloric After dephosphorization reaction, the content of phosphorus in iron ore complied completely with the requirements of steel production.
Keywords:high phosphorus  iron ore  dephosphorus  selective leaching  hydrochloric acid  dephosphorization ratio
本文献已被 维普 万方数据 等数据库收录!
点击此处可从《钢铁研究学报(英文版)》浏览原始摘要信息
点击此处可从《钢铁研究学报(英文版)》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号