Sensitization induced stress corrosion failure of AISI 347 stainless steel fractionator furnace tubes
Authors:J Swaminathan  Raghuvir Singh  Manoj Kumar Gunjan  Bhupeshwar Mahato
Affiliation:aMaterials Science and Technology Division, National Metallurgical Laboratory, Jamshedpur 831 007, India;bApplied Chemistry and Corrosion Division, National Metallurgical Laboratory, Jamshedpur 831 007, India
Abstract:Austenitic stainless steel tubes are used as furnace tubes in petrochemical industries mainly because of their corrosion resistance and mechanical strength. AISI 347 grade stainless steel is used as furnace heater tubes in the fractionator of hydrocracker unit. Even though this stainless steel is stabilized with the addition of niobium thus preventing sensitization related corrosion failures, operational and maintenance errors may result in premature failures if conditions prevail. The present work reports the premature failure of AISI 347 grade fractionator furnace tubes after nearly 8 years of service. The failure occurred after shutdown. Carbonaceous deposits were found on the inner walls of the tube and circumferential cracks were found beneath the deposit. The service exposed 347 SS alloy tube was in the sensitized condition as confirmed by microstructure and double loop electrochemical potentiodynamic reactivation test. The tube material got sensitized possibly by localized overheating at the carbon layer deposited site. During shutdown of hydrocracker unit polythionic acid formation occurred possibly due to errors in shutdown procedures. Sensitized alloy 347 tube undergone polythionic acid induced intergranular stress corrosion cracking (PASCC).
Keywords:Polythionic acid induced stress corrosion cracking  AISI 347 SS  Sensitization  Furnace tube failure
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号