The influence of compression failure on the bending, impact bending and tensile strength of spruce wood and the evaluation of non-destructive methods for early detection
Authors:W Sonderegger  P Niemz
Affiliation:1. Chair of Wood Science, Swiss Federal Institute of Technology (ETH), R?mistrasse 101, 8092, Zurich, Switzerland
Abstract:Bending strength (MOR) and bending Young’s modulus (MOE) according to DIN 52186 and MOE calculated on the basis of eigenfrequency and sound velocity were tested on small clear wood specimens of Norway spruce wood with and without compression failure. One group of specimens was climatised in a normal climate of 20°C and 65% relative humidity, while the other group was stored for one month under water before testing. The MOR of specimens with compression failure decreased about 20% on average (normal climate and wet) compared with the specimens without compression failure. The MOE of the specimens with compression failure was reduced only minimally compared with the specimens without compression failure stored in a normal climate, but very distinct differences (more then 30%) were found under wet conditions. The MOE of the specimens with compression failure calculated on the basis of eigenfrequency and sound velocity were not reduced or only minimally compared with the specimens without compression failure. It is therefore not possible to detect compression failure and to determine reduction in MOR using eigenfrequency or sound velocity. In addition, impact bending (DIN 52189), tensile strength and tensile MOE (DIN 52188) were tested on small clear wood specimens of Norway spruce wood with and without compression failure. The specimens with compression failure revealed an average reduction in impact strength of about 40% and an average reduction in tensile strength of about 20% compared with the specimens without compression failure, whereas tensile MOE of the specimens with compression failure was not reduced compared with the specimens without compression failure. The detection of compression failure by computer tomography (CT) was tested on Norway spruce wood boards 10 cm in thickness, and detection by optical scanner was tested on planed Norway spruce wood boards. CT recognised large compression failures easily, whereas the scanner was not able to detect them.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号