摘    要:采用激光诱导燃烧合成连接方法实现Cf/Al复合材料和TC4钛合金的可靠连接.放热中间层的燃烧合成反应为连接过程提供所需能量.结合理论计算和实验,对Ni?Al?Zr中间层的化学成分进行优化设计,并对连接接头的显微组织和力学性能进行研究.结果表明,Zr的加入轻微降低中间层的放热性,但显著提高连接质量,是实现可靠连接的关键....

关 键 词:Cf/Al复合材料  TC4钛合金  燃烧合成连接  界面显微组织  剪切强度
收稿时间:2021-02-21

Laser-induced combustion joining of Cf/Al composites and TC4 alloy
Affiliation:1. State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China;2. College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China
Abstract:The Cf/Al composites were joined to the TC4 alloy via the laser-induced combustion joining method. The exothermic reaction of the interlayer provided the required energy for the joining process. By combining the theoretical calculation and experiment, the chemical composition of the Ni–Al–Zr interlayer was designed. The microstructure and mechanical properties of the joint were investigated. The results show that the addition of Zr slightly weakened the combustion reaction of exothermic interlayer but played a key role in the successful joining. Ni–Al–Zr interlayer reacted with substrates, forming a TiAl3 layer adjacent to TC4 alloy and NiAl3, Ni2Al3 layers adjacent to the Cf/Al composites. Zr content dominated the microstructure and shear strength of the joint. When the Zr content was 5 wt.% under the joining pressure of 2 MPa, the joint had a maximum shear strength of 19.8 MPa.
Keywords:TC4 alloy  combustion joining  interfacial microstructure  shear strength