POC型气柜侧板纵焊缝开裂原因分析及处理
引用本文:郭亮,肖冬梅. POC型气柜侧板纵焊缝开裂原因分析及处理[J]. 冶金动力, 2002, 0(4): 33-34,40
作者姓名:郭亮  肖冬梅
作者单位:韶关钢铁集团公司动力厂,广东韶关,512123
摘    要:介绍了POC型气柜的结构,并从几个方面分析了韶钢POC钢干式煤气柜侧板内、外纵焊缝开裂的原因,并提出了一些具体的解决办法。

关 键 词:POC型 气柜 侧板纵焊缝 开裂 处理 煤气柜 高炉
文章编号:1006-6764(2002)04-0033-03

Causes Analysis of Cracking of the Vertical Weld Joints of the POC Gas-Holder Lateral Plate and the Solutions
GUO Liang,XIAO Dong mei. Causes Analysis of Cracking of the Vertical Weld Joints of the POC Gas-Holder Lateral Plate and the Solutions[J]. Metallurgical Power, 2002, 0(4): 33-34,40
Authors:GUO Liang  XIAO Dong mei
Abstract:Structure of the POC gas holder was presented. Causes of cracking of the internal and external vertical weld joints of the POC dry gas holder of Shaoguan Iron &Steel Co. were analyzed from several aspects. The practical solutions were given.
Keywords:gas holder  vertical weld joint of lateral plate  cracking  analysis  treatment