硅粉/酚醛制备低成本碳化硅陶瓷复合材料
引用本文:简科,胡海峰,陈朝辉. 硅粉/酚醛制备低成本碳化硅陶瓷复合材料[J]. 材料开发与应用, 2002, 17(6): 12-14
作者姓名:简科  胡海峰  陈朝辉
作者单位:国防科技大学新型陶瓷纤维及复合材料国防科技重点试验室,长沙,410073
摘    要:以低成本的硅粉和酚醛为原料 ,采用浆料浸渍 热压成型 反应烧结法制备了Cf SiC单向板 ,并对工艺条件进行了探讨。制备得到的单向板的弯曲强度达到 45 6 .8MPa ,断裂韧性达到 7.94MPa·m1 2 。

关 键 词:Cf/SiC单向板  硅粉  酚醛  复合材料
文章编号:1003-1545(2002)06-0012-03
修稿时间:2002-05-20

Fabrication of Low-cost Cf/SiC Composite from Silicon Powder and Phenolic Resins
Jian Ke Hu Haifeng Chen Zhaohui. Fabrication of Low-cost Cf/SiC Composite from Silicon Powder and Phenolic Resins[J]. Development and Application of Materials, 2002, 17(6): 12-14
Authors:Jian Ke Hu Haifeng Chen Zhaohui
Abstract:In order to get the low-cost SiC ceramic matrix, silicon powder and phenolic resins are adopted to fabricate C f/SiC unidirectional laminate by impregnation-hot pressing-pyrolysis sintering. The effect of process parameter on the performance is investigated. The maximum flexure strength and fracture toughness of the fabricated C f/SiC unidirectional laminate reach 456.8MPa and 7.94 MPa·m 1/2 respectively.
Keywords:C f/SiC unidirectional laminate Si powder Phenolic resin Composite