Abstract:Cotton–spun yarns from 34 staple stocks were manufactured by means of the ring–spinning process (34 yarns) and a rotor–spinning process (29 yarns) and tested for hairiness with the Shirley Hairiness Meter. For each spinning system, yarns were spun at two values of yarn linear density (15 and 30 tex for ring–spinning and 30 and 50 tex for rotor–spinning), but the twist multiplier was kept constant within the series for each spinning process.

The higher hairiness of ring–spun yarns and an increase ln hairiness with the yarn linear density were confirmed. The effect of the fibre parameters on yarn hairiness explains only about 30% of the total effect for ring–spun yarns and 40% for rotor–spun yarns. Fibre length and its uniformity are the fibre properties having the greatest influence on the hairiness of both ring– and rotor–spun yarns, the Micronaire index having only slight influence on the hairiness of ring–spun yarn.
Keywords:Short fibre  fibre length  fibre fineness  maturity ratio  fibre shedding  knitting