Dehydrogenation of Hydrogenated Ti-6Al-4V Alloy
Authors:Yuan Baoguo  Liu Dahai  Li Chunfeng
Affiliation:National Defence Key Discipline Laboratory of Light Alloy Processing Science and Technology, Nanchang Hangkong University, Nanchang 330063, China
Abstract:TG/DSC tests of non-hydrogenated and hydrogenated Ti-6Al-4V alloys were carried out in order to investigate the dehydrogenation behavior of hydrogenated titanium alloys. Results indicate that mass losses of the hydrogenated Ti-6Al-4V alloys are significantly different with that of the non-hydrogenated Ti-6Al-4V alloy when the heating temperature is higher than 600 oC. Mass loss of the hydrogenated Ti-6Al-4V alloy increases with the increasing of hydrogen content when the heating temperature is in the range of 600 oC to 900 oC due to the decomposition of metastable phases. The maximum mass loss of the hydrogenated Ti-6Al-4V alloy is in correspondence with its hydrogen content upon no consideration of oxidation. The optimal dehydrogenation temperature among hydrogenated Ti-6Al-4V alloys is 750 oC. The dehydrogenation process for all hydrogenated Ti-6Al-4V alloys is the same
Keywords:titanium alloy   hydrogen   dehydrogenation   TG/DSC
本文献已被 CNKI 等数据库收录!
点击此处可从《稀有金属材料与工程》浏览原始摘要信息
点击此处可从《稀有金属材料与工程》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号