Q235B热轧板表面纵裂成因分析及工艺控制
引用本文:张瑜,漆鑫,杨春雷,张红斌.Q235B热轧板表面纵裂成因分析及工艺控制[J].特殊钢,2016,37(1):29-33.
作者姓名:张瑜  漆鑫  杨春雷  张红斌
作者单位:1武钢集团昆明钢铁股份有限公司技术中心,昆明650302; 2昆明理工大学,昆明650093
摘    要:Q235B钢(0. 11% ~0. 17%C)10~20 mm热轧板的生产流程为铁水预处理-50 t转炉-吹氧-(2。0 ~ 230)mm x(900 ~ 1 600)mm板坯连铸-热轧工艺。分析表明.Q235B钢热轧板表面裂纹来源于铸坯纵裂。统计分 析了成分、钢水过热度、拉速、连铸二冷水量、保护渣等对连铸坯纵裂的影响。通过控制Mn/S≥40,钢水过热度 15-35 °C,拉速1. 15 m/min,按季节调节二冷水量,釆用熔点≥1 100 °C,粘度0.20 ~0. 32 Pa .s,碱度≥1. 10的保 护渣等措施,使Q235B钢热轧板表面纵裂纹由3.51%降至W0. 96%。

关 键 词:Q235B钢  热轧板  表面纵裂  Mn/S     200mm板坯  过热度  拉速  保护渣  
收稿时间:2015-08-05

Analysis on Forming Cause of Surface Longitudinal Crack of Steel Q235B Hot-Rolled Plate and Controlling Process
Zhang Yu,Qi Xin,Yang Chunlei,Zhang Hongbin.Analysis on Forming Cause of Surface Longitudinal Crack of Steel Q235B Hot-Rolled Plate and Controlling Process[J].Special Steel,2016,37(1):29-33.
Authors:Zhang Yu  Qi Xin  Yang Chunlei  Zhang Hongbin
Affiliation:1 Technology Center, Kunming Iron and Steel Co Ltd, Wuhan Iron and Steel Group, Kunming 650302;
2 Kunming University of Science and Technology, Kunming 650093
Abstract:The flowsheet for 10 ~20 mm hot-rolled plate of Q235B steel (0. 11% ~0. 17% C) is hot metal pretreatment-50 t converter-argon blowing-(200 ~230)mm x (900 ~ 1 600) mm slab casting-hot rolling process. The analysis results show that the surface crack of hot-rolled plate stems from casting slab longitudinal cracks of steel Q235B. The effect of composition, liquid overheat extent, casting speed, casting secondary water rate and mold powder on longitudinal crack of casting slab has been statistically analyzed. With the measures including controlling Mn/S ≥40, liquid overheat extent 15 ~35 °C , casting speed 1. 15 m/min, adjusting secondary water rate according to season and using mold powder with melting point ≥1 100°C , viscosity 0. 20 ~ 0. 32 Pa .s and basicity ≥1. 10, the ratio of occurrence of steel Q235B hot- rolled plate surface longitudinal crack decreases to ≤0. 96% from original 3. 51% .
Keywords:
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《特殊钢》浏览原始摘要信息
点击此处可从《特殊钢》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号