首页 | 本学科首页   官方微博 | 高级检索  
     

火焰原子吸收光谱法测定红土镍矿中铜含量
引用本文:李昌丽,蒋晓光,汤淑芳,刘春峰,李华昌,张彦甫,褚 宁. 火焰原子吸收光谱法测定红土镍矿中铜含量[J]. 冶金分析, 2012, 32(10): 74-77
作者姓名:李昌丽  蒋晓光  汤淑芳  刘春峰  李华昌  张彦甫  褚 宁
作者单位:1.鲅鱼圈出入境检验检疫局,辽宁营口 115007;2.北京矿冶研究总院,北京100044
摘    要:

关 键 词:火焰原子吸收光谱法  红土镍矿    
收稿时间:2012-01-30

Determination of copper in laterite nickel oreby flame atomic absorption spectrometry
LI Chang-li,JIANG Xiao-guang,TANG Shu-fang,LIU Chun-feng,LI Hua-chang,ZHANG Yan-fu,CHU Ning. Determination of copper in laterite nickel oreby flame atomic absorption spectrometry[J]. Metallurgical Analysis, 2012, 32(10): 74-77
Authors:LI Chang-li  JIANG Xiao-guang  TANG Shu-fang  LIU Chun-feng  LI Hua-chang  ZHANG Yan-fu  CHU Ning
Affiliation:1. Bayuquan Entry-Exit Inspection and Quarantine, Yingkou 115007, China;2. Beijing General Research Institute of Mining & Metallurgy, Beijing 100044, China
Abstract:The laterite nickel ore sample was decomposed with hydrochloric acid, nitric acid, hydrofluoric acid and perchloric acid. Then, in diluted nitric acid medium, the content of copper was determined on flame atomic absorption spectrometry at 324.8 nm. The background was deducted with deuterium lamp. Under optimized experimental conditions, the absorbance is linear with copper concentration in the range of 0.50-2.50 mg/L. The limit of determination was 0.057 mg/L. The recoveries obtained by standard addition method range from 91% to 103%.Copper content range from 0.01% to 0.50%, the equation of repeatability and reproducibility are r=0.114 8m+0.003 2 and R=0.130 0 m+0.007 4. This method was applicable for the determination of laterite nickel ore with copper content of 0.01%-0.50%.
Keywords:flame atomic absorption spectrometry  laterite nickel ore  copper  
点击此处可从《冶金分析》浏览原始摘要信息
点击此处可从《冶金分析》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号