Study on thickness loss of cut-pile carpet produced with heat process modified polyester pile yarn. Part II: dynamic loading
Authors:M Javidpanah  S Shaikhzadeh Najar
Affiliation:1. Department of Textile Engineering, Science &2. Research Branch, Islamic Azad University, Tehran, Iran;3. Department of Textile Engineering, Amirkabir University of Technology, Tehran, Iran
Abstract:Thickness loss (TL) is one of the most important mechanical properties in each carpet. In this research, four types of ATY polyester pile yarns were used to prepare the cut-pile carpet samples. They were normal ATY polyester filament pile yarns and three yarns that modified by heat processes including friezing, heat setting, and twist heat setting. Woven carpet samples are subjected to standard dynamic loading test. Results show that friezing and heat setting processes have no significant effects on carpet dynamic recovery or TL after dynamic loading. Also, decreasing temperature of twist heat setting, the polyester pile yarns could not modify carpet TL after dynamic loading.
Keywords:carpet  air-jet textured (ATY) polyester filament pile yarn  dynamic loading  thickness loss  heat process
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号