摘    要:本文简要介绍了国外研制6.5%Si钢的历史及最新进展,着重对已有产品面市的日本NKK公司的CVD法的工艺技术及设备状况进行了综述。

关 键 词:6.5%Si钢  化学气相沉积(CVD)  磁场冷却

PROCESS AND EQUIPMENT OF CVD METHOD FOR 6. 5% SILICON STEEL
Wang Xiangcheng Scientific and Technological Information Research Institute WISCO. PROCESS AND EQUIPMENT OF CVD METHOD FOR 6. 5% SILICON STEEL[J]. Research on Iron and Steel, 1992, 0(5)
Authors:Wang Xiangcheng Scientific and Technological Information Research Institute WISCO
Affiliation:Wang Xiangcheng Scientific and Technological Information Research Institute WISCO
Abstract:A brief introduction was made to the history and recent progress in the research and development of 6. 5% silicon steel abroad. Emphasis was laid upon a review of the process and equipment of CVD method invented by NKK Japan, who has now had ready made products of the steel on the market.
Keywords:6. 5 % silicon steel  chemical vapour deposition  magnetic-field cooling