摘    要:首先研究了细骨料携带不同质量分数氯离子的砂浆试件在3,5,7,14,28,90d的抗折、抗压强度的变化规律,发现与拌制用水中携带氯离子具有早强作用不同,细骨料携带氯离子不但不会引起早强,反而会降低强度。基于4年的长期暴露试验,系统研究细骨料携带不同质量分数氯离子的砂浆试件在270,360,450,630,810,105...

关 键 词:细骨料携带氯离子  长期暴露试验  抗压抗折强度  粘结性能  氯离子含量

LONG-TERM EXPOSURE EXPERIMENTAL INVESTIGATION ON MORTAR STRENGTH AND ITS BOND PERFORMANCE WITH CHLORIDE ION PERMEATING IN SANDS
Zhang Xiaogang,Wang Weilun,Wang Jiao,Yang Rui.LONG-TERM EXPOSURE EXPERIMENTAL INVESTIGATION ON MORTAR STRENGTH AND ITS BOND PERFORMANCE WITH CHLORIDE ION PERMEATING IN SANDS[J].Industrial Construction,2011,41(5):1-5.
Authors:Zhang Xiaogang  Wang Weilun  Wang Jiao  Yang Rui
Affiliation:Zhang Xiaogang Wang Weilun Wang Jiao Yang Rui (Shenzhen Municipal Key Laboratory for Durability of Civil Engineering Structure,College of Civil Engineering,Shenzhen University,Shenzhen 518060,China)
Abstract:Firstly,the compressive and flexural strength of mortar with chloride ion permeating in sands during mixing investigated in 3,5,7,14,28,and 90 d.It is found that chloride ion permeating in sands will not improve the mortar strength of early stage,but reduce the corresponding strength,which is obviously different from the effect of chloride ion permeating in water.Then the bond performance of above mortar in 270,360,450,630,810,1 050,1 170,1 320,and 1 440 d was studied based on 4 years long-term exposure experiments.The τ-s slipping curve with different content of chloride ion,the time-variant maximal bonding strength,also its tensility change rule are presented.Finally,the fitting formula of τ-s was gained by origin software.
Keywords:chloride ion permeating in sands  long-term exposure experiment  compressive and flexural strength  bond performance  content of chloride ion