Residual stress measurement on propellant tank of 2219 aluminum alloy and study on its weak spot
Authors:Chaoqun Huang  Huan Li  Jianxiong Li  Chuanguang Luo  Yanbing Ni
Affiliation:1.School of Materials Science and Engineering, Tianjin Key Laboratory of Advanced Joining Technology,Tianjin University,Tianjin,China;2.Sichuan Institute of Aerospace Systems Engineering,Chengdu, Sichuan,China;3.School of Mechanical Engineering,Tianjin University,Tianjin,China
Abstract:This paper presented residual stress measurement on two circumferential Variable polarity plasma arc welding (VPPAW) joints and one circular closed Friction stir welding (FSW) joint on the propellant tank of 2219 aluminum alloy using the indentation strain-gauge method. Quite large tensile residual stresses were attached to the center and inner areas of the circular closed FSW joint. There were very large tensile stresses in some points of the two circumferential VPPAW joints, among these points, the maximum value was +253 MPa, which was about 63 % of the yield strength of 410 MPa measured in the base material. In addition, the peak of compressive residual stress was about -160 MPa. Above all, there were two typical peaks of residual stress in the circumferential VPPAW joints, one was located in the middle part while the other one was near the start/end position of the joints. Combining the result of residual stress measurement with the characteristics of the tank structure, it can be concluded that circular closed FSW joint around the flange was a weak spot on the propellant tank. And the most vulnerable point on the circular closed FSW joint has also been found.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号