Influence of flow control devices on metallurgical effects in a large—capacity tundish
引用本文:CaijunZhang WeixiaYuan 等.Influence of flow control devices on metallurgical effects in a large—capacity tundish[J].北京科技大学学报(英文版),2002,9(6):412-416.
作者姓名:CaijunZhang  WeixiaYuan
作者单位:[1]MetallurgyEngineeringSchool,UniversityofScienceandTechnologyBeijing,Beijing100083,China [2]WuhanIronandSteel(Group)Corp.,Wuhan430080,China
摘    要:The influence of flow control devices on metallurgical effects in large-capacity tundish has been studied carefully with elements tracing,sampling and theoretical prospecting,The results from the studies are(1) in the continuous casting of clean steel,bad control of tundish operation may deteriorate the cleanliness of steel;(2) the cleanliness of steel is deteriorated mainly at the unstady state;(3) large amount of macro inclusions come from the top slag and the refractory of tundish;(4) installing dam and weir can improve the cleanliness of steel and lighten the influence of steel fluctuation;and (5) the result of theoretical calculation suggests that the inclusions larger than the critical size of 92.6um can be floated out from the tundish bath completely.

关 键 词:精炼钢  射流控制器件  冶金效率

Influence of flow control devices on metallurgical effects in a large-capacity tundish
Caijun Zhang,Lin Wang,Kaike Cai,Weixia Yuan,Zhixiang Yu,Yang Zou.Influence of flow control devices on metallurgical effects in a large-capacity tundish[J].Journal of University of Science and Technology Beijing,2002,9(6):412-416.
Authors:Caijun Zhang  Lin Wang  Kaike Cai  Weixia Yuan  Zhixiang Yu  Yang Zou
Affiliation:1. Metallurgy Engineering School, University of Science and Technology Beijing, Beijing 100083, China
2. Wuhan Iron and Steel Group Corp., Wuhan 430080, China
Abstract:The influence of flow control devices on metallurgical effects in a large-capacity tundish has been studied carefully with elements tracing, sampling and theoretical prospecting. The results from the studies are (1) in the continuous casting of clean steel, bad control of tundish operation may deteriorate the cleanliness of steel; (2) the cleanliness of steel is deteriorated mainly at the unsteady state; (3) large amount of macro inclusions come from the top slag and the refractory of tundish; (4) installing dam and weir can improve the cleanliness of steel and lighten the influence of steel fluctuation; and (5) the result of theoretical calculation suggests that the inclusions larger than the critical size of 92.6 μm can be floated out from the tundish bath completely.