Abstract:A series of novel thermoplastic elastomers, based on poly(dimethylsiloxane) (PDMS) as the soft segment and poly(butylene terephthalate) (PBT) as the hard segment, were synthesized by catalyzed two‐step, melt transesterification reactions of dimethyl terephthalate and methyl esters of carboxypropyl‐terminated poly(dimethylsiloxane)s (M?n = 550–2170 g mol?1) with 1,4‐butanediol. The lengths of both the hard and soft segments were varied while the weight ratio of the hard to soft segments in the reaction mixture was maintained constant (57/43). The molecular structure, composition and molecular weights of the poly(ester–siloxane)s were examined by 1H NMR spectroscopy. The effectiveness of the incorporation of the methyl‐ester‐terminated poly(dimethylsiloxane)s into the copolymer chains was verified by chloroform extraction. The effect of the segment length on the transition temperatures (Tm and Tg) and the thermal and thermo‐oxidative degradation stability, as well as the degree of crystallinity and hardness properties of the synthesized TPESs, were studied. Copyright © 2003 Society of Chemical Industry
Keywords:poly(ester–  siloxane)s  thermoplastic elastomers  carboxypropyl‐terminated poly(dimethylsiloxane)s
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号