摘 要: | 采用Gleeble 1500热模拟试验机对SAE8640钢280 mm×325 mm连铸坯(/%:0.41C,0.20Si,0.80Mn,0.005S,0.014P,0.46Cr,0.43Ni,0.21Mo,0.043Alt,0.001 10,0.005 4N)的550~1 200℃力学性能进行了测定,并应用扫描电镜观察了拉力试样的断口形貌。结果表明,SAE8640钢有明显的3个脆性区:Ⅰ脆性区1 200℃,Ⅱ脆性区950~1 000℃,Ⅲ脆性区650~750;该钢950~1 000℃的断面收缩率为60%,拉伸断口为脆性河流状花样,应避免在该温度范围进行轧制,该钢650~750℃的断面收缩率≥65%,拉伸断口为韧性断裂,可满足连铸坯矫直时塑性的要求。
|