Abstract: | A series of liquid crystalline aromatic polyesters containing 3,3′-dimethylbiphenyl-4,4′-dicarboxylic acid and 3,4′-dimethyl-biphenyl-4,3′-dicarboxylic acid was prepared by a melt polycondensation procedure and characterized by elemental analysis, DSC and TMA measurements, and optical polarizing microscopy. An optimal composition of the copolymer having a melting temperature around 300°C is proposed and the rheological behavior is discussed. Most of the mechanical properties of this copolymer were found to be close to those of Vectra A950® used as a reference sample. © 1996 John Wiley & Sons, Inc. |