摘    要:以乙氧化双酚A二甲基丙烯酸酯(BPA2EODPT)、环氧丙烯酸酯(EA)和三羟甲基丙烷三甲基丙烯酸酯(TMPTMA)为主要原料,N,N'-4,4'-二苯甲烷双马来酰亚胺(BMI)和气相二氧化硅(SiO2)为耐热改性剂,异丙苯过氧化氢(CHP)为引发剂,N,N-二乙基对甲苯胺(DPT)和糖精(SA)为促进剂和助促进剂,对苯醌(BQ)、乙二胺四乙酸四钠(Na4EDTA)和对苯二酚(HQ)为稳定剂,优选出耐高温厌氧胶的最佳配方。结果表明:当m(BPA2EODPT)︰ m(EA)︰m(TMPTMA)=3.1︰1︰2.5、w(BMI)=6%、w(SiO2)=4%、w(CHP)=3.5%、w(DPT)=0.4%、w(SA)=2%、w(BQ)=0.07%、w(Na4EDTA)=0.04%、w(HQ)=0.11%时,厌氧胶的综合性能较好,耐热性能及贮存稳定性能俱佳。

关 键 词:厌氧胶  耐高温  贮存稳定性  扭矩强度  热老化强度

Preparation of high temperature resistant anaerobic adhesive and its storage life
PENG Xiaoqin,CHEN Liang,CHEN Bingyao,LING Hui,LI Jun. Preparation of high temperature resistant anaerobic adhesive and its storage life[J]. Chemical Industry and Engineering Progress, 2012, 31(9): 2058-2063
Authors:PENG Xiaoqin  CHEN Liang  CHEN Bingyao  LING Hui  LI Jun
Affiliation:1Guangdong SANVO Chemical Technology Co.Ltd.,Zhongshan 528429,Guangdong,China;2Foshan FUTIM Coating Chemical Co.Ltd.,Foshan 528325,Guangdong,China;3Zhongshan FUHE Chemical Technology Co.Ltd.,Zhongshan 528434,Guangdong,China
Abstract:With ethoxylated bisphenol A dimethacrylate (BPA2EODPT) and epoxy acrylate (EA) and trimethylolpropane trimethacrylate (TMPTMA) as raw materials,N,N'-4,4'- diphenylmethyenebismaleimide (BMI) and gas phase silicon dioxide(SiO2) as heat resistant modifier,cumene hydroperoxide (CHP) as initiator,N,N-diethyl-p-toluidine and saccharin as main accelerant and secondary accelerant respectively, p-benzoquinone (BQ) and tetrasodium EDTA (Na4EDTA) and hydroquinone (HQ) as stabilizer,the formula of anaerobic adhesive was optimized. The properties of the anaerobic adhesive were better because of its good heat resistance and storage stability when mass ratio of m(BPA2EODPT)︰m(EA)︰m(TMPTMA) was 3.1︰1︰2.5,mass fractions of BMI and SiO2 were 6% and 4% respectively,mass fractions of DPT and SA were 0.4% and 2% respectively,mass fractions of BQ and Na4EDTA and HQ were 0.07% and 0.04% and 0.11% respectively.
Keywords:anaerobic adhesive  high temperature  heat resistance  torque strength  storage stability
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《化工进展》浏览原始摘要信息
点击此处可从《化工进展》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号