烧结炉中20g钢冷却管爆裂分析
引用本文:张小球 潘珊珊. 烧结炉中20g钢冷却管爆裂分析[J]. 上海金属, 1995, 17(6): 48-52
作者姓名:张小球 潘珊珊
作者单位:上海第三钢铁厂!200126
摘    要:对烧结炉中20g钢冷却管爆裂所进行的检验确认爆裂原因是冷却水量小及水质差引起堵塞,造成过热过烧。建议软化水质和改进冷却系统为解决途径。

关 键 词:烧结炉 冷却管 失效分析 冷却水

THE ANALYSIS FOR BURSTING OF 20g STEEL FOR COOLING PIPE IN SINTERING FURNACE
Zhang Xiaoqiu, Pan Shanshan, Fan Liyu. THE ANALYSIS FOR BURSTING OF 20g STEEL FOR COOLING PIPE IN SINTERING FURNACE[J]. Shanghai Metals, 1995, 17(6): 48-52
Authors:Zhang Xiaoqiu   Pan Shanshan   Fan Liyu
Affiliation:Shanghai No. 3 Steel Works
Abstract:The bursting of 20g steel for cooling pipe in sintering furnace was the result of pipe blocking, over-heating and over-burning caused by inferior water quality and inadequate water quantity. The proposed solution is to soften the water and improve the cooling system.
Keywords:Cooling pipe for sintering furnace   Failure Analysis   Cooling Water