摘    要:通过对CO2气保药芯焊丝堆进行焊工艺试验发现,焊接电流、干伸长度、搭接量(S)三个工艺参数制定不当,是导致堆焊层侧弯不合格的重要因素。同时对CO2气保药芯焊丝堆焊的主要工艺参数进行了分析说明,确定了不锈钢CO2气保药芯焊丝堆焊的最佳焊接工艺规范参数。

关 键 词:CO2气保药芯焊丝堆焊  侧弯  焊接电流  干伸长度  搭接量(S)  

Analysis cladding welding with side-bend unqualified of FCAW with CO2 gas-shielded
WANG Tian-xian. Analysis cladding welding with side-bend unqualified of FCAW with CO2 gas-shielded[J]. Electric Welding Machine, 2010, 40(2)
Authors:WANG Tian-xian
Affiliation:Qingdao LS Heavy Machinery Equipment Co.;Ltd.;Qingdao 266426;China
Abstract:This article according to the welding process experiment of FCAW with CO2 gas shielded shows that welding current,stick- out,overlap (S),are the main welding parameters which lead to overlay side-bend unqualified of FCAW with CO2 gas-shielded.By analysing the welding parameters,we definite the best welding parameters for FCAW with CO2 gas shielded.
Keywords:FCAW with CO2 gas shield  side-bend  welding current  stick-out  the mount of overlay  