摘    要:The effect of hydrogen on hot deformability of Ti-6Al-4V alloy was investigated by isothermal hot compression test with temperature of 800 ℃ and velocity of 0.1 mm/s. By optical microscopy (OM) and transmission electron microscopy (TEM), the influence of hydrogen on the microstructural features was systematically examined including the morphology of a grain, volume fraction of a phase and dynamic recrystallization (DRX). The flow stress shows an initial decrease but a later increase with the increase of hydrogen content. The minimum of peak compression flow stress is obtained when 0.2% hydrogen is added into the alloy. The hydrogen-induced softening of Ti-6Al-4V alloy may be that hydrogen induces the increase of proportion of soft β phase, the increase of DRX and the increase of extent of twins.

关 键 词:钛合金 氢 可加工性 变形性 再结晶作用
收稿时间:2006-07-28
修稿时间:2006-09-15

Hydrogen-induced hot workability in Ti-6Al-4V alloy
ZONG Ying-ying, SHAN De-bin , LU Yan, GUO Bin. Hydrogen-induced hot workability in Ti-6Al-4V alloy[J]. Transactions of Nonferrous Metals Society of China, 2006, 16(A03): 2072-2076
Authors:ZONG Ying-ying   SHAN De-bin    LU Yan   GUO Bin
Abstract:
Keywords:
本文献已被 维普 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号