Ca^2+,Mg^2+对黑钨矿选择性絮凝的影响及其机理研究
引用本文:杨久流,李颖.Ca^2+,Mg^2+对黑钨矿选择性絮凝的影响及其机理研究[J].矿冶,1998,7(1):29-32.
作者姓名:杨久流  李颖
作者单位:北京矿冶研究总院,中国矿业大学北京研究生部,北京有色金属研究总院
摘    要:矿浆中Ca2+、Mg2+的含量显著影响黑钨矿选择性絮凝效果。研究结果表明,Ca2+、Mg2+均是通过降低颗粒表面ζ 电位而使微细矿粒之间产生凝聚或互凝,添加适量的Na2CO3可克服矿浆中Ca2+、Mg2+的不良影响。在配水中,以FD为絮凝剂、(NaPO3)6为分散剂,可实现黑钨矿与4种脉石矿物人工混合矿的分离。

关 键 词:微细粒黑钨矿  选择性絮凝

EFFECTS OF Ca~2+ AND Mg~2+ ON SELECTIVE FLOCCULATION OF WOLFRAMITE AND ITS MECHANISM
Abstract:Selective flocculation of wolframite is considerably influenced by the content of Ca~2+ and Mg~2+ in pulp.Research results show that,both Ca~2+ and Mg~2+ can lower the Zeta potential on the surface of particles and cause the coagulation among fine particles.The bad effects of Ca~2+ and Mg~2+ in pulp can be overcome by adding the right amount of Na_2CO_3.In the condition of FD used as flocculant and (NaPO_3)_6 as dispersant,wolframite can be separated from four kinds of gangue minerals in mixed water.
Keywords:Wolframite fine  Selective flocculation