首页 | 本学科首页   官方微博 | 高级检索  
     

棉/涤皮芯结构粗纱参数对其细纱结构与性能的影响
引用本文:郭明瑞,顾银华,高卫东.棉/涤皮芯结构粗纱参数对其细纱结构与性能的影响[J].纺织学报,2022,43(6):57-62.
作者姓名:郭明瑞  顾银华  高卫东
作者单位:生态纺织教育部重点实验室(江南大学), 江苏 无锡 214122
基金项目:国家自然科学基金青年基金项目(52003105);江苏省博士后科研资助计划项目(2020Z140B)
摘    要:为探究皮芯粗纱参数对粗纱—细纱两步法纺制棉/涤皮芯结构短纤纱的外观形貌及性能的影响,研究皮芯粗纱纺纱工艺、粗纱定量、粗纱捻度,以及芯纤维含量等因素对棉/涤皮芯结构短纤纱的芯纤维外露比例和纱线性能的影响规律。并借助图像处理技术,实现了芯纤维外露比例的定量化测试。结果表明:当粗纱工序输出须条宽度由10.2 mm增至16.3 mm,皮芯粗纱中芯纤维束偏心度由26.5%降低至19.2%,细纱芯纤维外露比例降低11.3%(29.2 tex)和12.3%(19.4 tex);粗纱定量增大或捻系数减小,芯纤维外露比例降低;芯纤维涤纶含量由15%增加至25%,芯纤维外露比例增加35.6%(29.2 tex)和30.5%(19.4 tex)。

关 键 词:皮芯结构短纤纱  芯纤维含量  芯纤维外露比例  粗纱  细纱  
收稿时间:2021-04-05

Influence of cotton/polyester sheath-core structure roving parameters on structure and performance of spun yarn
GUO Mingrui,GU Yinhua,GAO Weidong.Influence of cotton/polyester sheath-core structure roving parameters on structure and performance of spun yarn[J].Journal of Textile Research,2022,43(6):57-62.
Authors:GUO Mingrui  GU Yinhua  GAO Weidong
Affiliation:Key Laboratory of Eco-Textiles(Jiangnan University), Ministry of Education, Wuxi, Jiangsu 214122, China
Abstract:In order to investigate the influence of roving parameters on the appearance and properties of cotton/polyester sheath-core staple yarns by the two-step spinning process, the effects of factors such as spinning settings, roving linear density, roving twist and core/sheath fiber ratio on the exposure of core fiber and yarn properties were studied. With the help of image processing technology, the core fiber exposure ratio was quantitatively measured. The results show that as the width of fiber bundle output from roving frame increases from 10.2 mm to 16.3 mm, the eccentricity of core fiber bundle in roving decreases from 26.5% to 19.2%, and the exposure ratio of core fiber in yarn decreases by 11.3% (29.2 tex) and 12.3% (19.4 tex). When the roving count increases or the twist coefficient decreases, the core fiber exposure proportion decreases. When the proportion of polyester core fiber increased from 15% to 25%, the exposure proportion of core fiber increased by 35.6% (29.2 tex) and 30.5% (19.4 tex).
Keywords:sheath-core staple yarn  core fiber ratio  core fiber exposure proportion  roving  spun yarn  
点击此处可从《纺织学报》浏览原始摘要信息
点击此处可从《纺织学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏