首页 | 本学科首页   官方微博 | 高级检索  
     

异型薄壁零件淬火畸变的控制
引用本文:李小银,崔军. 异型薄壁零件淬火畸变的控制[J]. 金属热处理, 2004, 29(3): 64-66
作者姓名:李小银  崔军
作者单位:重庆大江工业集团有限责任公司,重庆,401321
摘    要:分析了异型薄壁零件淬火废品率高的主要原因。采取改进工艺、工装设计及淬火后校正3方面措施,有效控制了该零件的淬火畸变,显著降低了零件淬火的废品率。

关 键 词:异型薄壁零件 淬火畸变 废品率
文章编号:0254-6051(2004)03-0064-03

Quenching Distortion Controlling of Special Shape and Thin Wall Parts
LI Xiao-yin,CUI Jun. Quenching Distortion Controlling of Special Shape and Thin Wall Parts[J]. Heat Treatment of Metals, 2004, 29(3): 64-66
Authors:LI Xiao-yin  CUI Jun
Abstract:The main reasons of high reject rate for the special shape and thin wall parts were analyzed.The quenching distortion of the parts was controlled effectively by improving the quenching process,the technology installations and the correcting after quenching.Consequently,the reject rate of the parts lowered greatly.
Keywords:special shape and thin wall parts  quenching distortion  reject rate  