Abstract:Compatibilization of the blends of polydimethyl siloxane (PDMS) rubber and low‐density polyethylene (LDPE) was achieved through reactive processing during extrusion in a Monsanto Processability Tester (MPT). The chemorheological characteristics of 50 : 50 LDPE : PDMS blends with varying proportions (0–8 wt %) of ethylene comethyl acrylate (EMA) were investigated at three different temperatures (170, 190, and 210°C) and four different shear rates (61.3, 122.6, 306.6, and 613.1 s?1). It was found that EMA reacts with vinyl groups of PDMS rubber at a temperature of 190°C during extrusion through the capillary of MPT, forming EMA‐grafted‐PDMS rubber (EMA‐g‐PDMS), which acts as the compatibilizer for the blend systems. The results are based on IR spectroscopy, melt rheology, and phase morphology of the blends. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 12: 2810–2817, 2003
Keywords:compatibilization  blends  rheology  morphology  infrared spectroscopy
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号