Coke burning behavior of a catalyst of ZSM-5/ZSM-11 co-crystallized zeolite in the alkylation of benzene with FCC off-gas to ethylbenzene |
| |
Affiliation: | 1. School of Chemistry and Materials Sciences, Research Institute of Crop Science, Heilongjiang University, Harbin 150080, China;2. Fushun Research Institute of Petroleum and Petrochemicals, SINOPEC, Fushun 113000, China |
| |
Abstract: | Since the commercialization of ethylbenzene production via alkylation of benzene with the dilute ethene in FCC off-gas over a ZSM-5/ZSM-11 co-crystallized zeolite catalyst in China, the catalyst has been regenerated several times and showed good regeneration performance. During the alkylation process, the catalytic activity decreases, some of the catalyst pores are blocked and the acid centers are partly covered by coke deposition. Influence of the factors such as catalyst particle size, temperature, etc. on the burning rate of the coke was investigated by the TG technique, and a rate equation for coke burning on the ZSM-5/ZSM-11 co-crystallized catalyst was established. |
| |
Keywords: | |
本文献已被 ScienceDirect 等数据库收录! |
|