Preparation of semi-solid aluminum alloy slurry poured through a water-cooled serpentine channel
Authors:Zheng-zhou Chen  Wei-min Mao  Zong-chuang Wu
Affiliation:School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
Abstract:A water-cooled serpentine channel pouring process was invented to produce semi-solid A356 aluminum alloy slurry for rheocasting,and the effects of pouring temperature and circulating cooling water flux on the microstructure of the slurry were investigated.The results show that at the pouring temperature of 640-680°C and the circulating cooling water flux of 0.9 m3/h,the semi-solid A356 aluminum alloy slurry with spherical primary α(Al) grains can be obtained,whose shape factors are between 0.78 and 0.86 and the grain diameter can reach 48-68 μm.When the pouting temperatures are at 660-680°C,only a very thin solidified shell remains inside the serpentine channel and can be removed easily.When the serpentine channel is cooled with circulating water,the microstructure of the semi-solid slurry can be improved,and the serpentine channel is quickly cooled to room temperature after the completion of one pouring.In terms of the productivity of the special equipment,the water-cooled serpentine channel is economical and efficient.
Keywords:semi-solid slurry  aluminum alloys  microstructure  rheocasting
本文献已被 CNKI 维普 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号