Low-temperature sol-gel intermediate layer wafer bonding
Authors:SS Deng  J Wei  H Xie
Affiliation:a School of Electrical and Electronic Engineering, Nanyang Technological University, 639798 Singapore
b Singapore Institute of Manufacturing Technology, 71 Nanyang Drive, 638075 Singapore
Abstract:Silicon-to-silicon wafer bonding has been successfully performed using sol-gel intermediate layer, which is deposited by spinning acid-catalyzed tetraethylthosilicate solution on the surfaces of two silicon wafers to be bonded. The bond strength is up to 35 MPa at a bonding temperature of 100 °C, which is near to the fractured strength of bulk silicon. To investigate the effects of the press parameters, Draper-Lin small composite design is used, as it requires the minimum number of runs in the design of experiments. Statistic analysis shows that the bonding temperature is the dominant factor for the bond quality, while the interaction between bonding temperature and concentration is significant on bond strength. The physical mechanisms of the observed significant effects are discussed. The improvement of the wafer bonding using annealed sol-gel intermediate layer is also proposed.
Keywords:81  20  Fw  81  20  Vj  07  05  Fb  82  30  Ra
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号