首页 | 本学科首页   官方微博 | 高级检索  
     

冷轧平整横折印缺陷产生原因和消除方法
引用本文:周正元,吴迪. 冷轧平整横折印缺陷产生原因和消除方法[J]. 轧钢, 2002, 19(2): 19-21
作者姓名:周正元  吴迪
作者单位:1. 上海益昌薄板有限公司技术部,上海,200431
2. 东北大学轧制技术及连轧自动化国家重点实验室,辽宁,沈阳,110004
摘    要:针对冷轧平整存在横折印问题进行了分析 ,找出其产生原因及消除方法 ,并研制了带V型槽和凸度的张紧辊。新张紧辊对减少横折印缺陷效果明显 ,缺陷数量可减少 99 2 %以上。

关 键 词:冷轧带钢  平整  横折印  V型槽  张紧辊
文章编号:1003-9996(2002)02-0019-03
修稿时间:2001-06-25

Study on the strip surface wrinkles and the elimination measures in cold temper rolling
ZHOU Zheng-yuan ,WU Di. Study on the strip surface wrinkles and the elimination measures in cold temper rolling[J]. Steel Rolling, 2002, 19(2): 19-21
Authors:ZHOU Zheng-yuan   WU Di
Affiliation:ZHOU Zheng-yuan 1,WU Di 2
Abstract:The causes of producing surface wrinkles of strip cold temper rolling were analyzed and the elimination measures were found out.The tension bridle rolls with convexity and V-type groove were developed, which have obvious effect to reduce defect amount to more than 99.2%.
Keywords:cold rolled strip  temper  wrinkles  V-type groove  tension bridle rolls
本文献已被 CNKI 维普 万方数据 等数据库收录!