首页 | 本学科首页   官方微博 | 高级检索  
     

唐钢FTSC工艺薄板坯连铸粘结的原因及预防措施
引用本文:马新光,张云飞. 唐钢FTSC工艺薄板坯连铸粘结的原因及预防措施[J]. 冶金标准化与质量, 2007, 45(3): 19-21
作者姓名:马新光  张云飞
作者单位:唐山钢铁集团股份有限公司第一钢轧厂,河北,唐山,063016
摘    要:通过结合唐钢薄板坯连铸的生产实践,从钢水纯净度及温度、结晶器内钢水液位波动、锥度控制、设备状况、保护渣性能等几个方面分析薄板坯连铸粘结的机理和影响因素,并提出相应的预防措施,使粘结几率有较大幅度的降低。

关 键 词:薄板坯连铸  粘结  措施
文章编号:1003-0514(2007)03-0019-03
修稿时间:2007-05-14

The reasons and preventive measures of Tangsteel''''s FTSC thin slab continuous casting bonding
MA Xin-guang,ZHANG Yun-fei. The reasons and preventive measures of Tangsteel''''s FTSC thin slab continuous casting bonding[J]. Metallurgical Standardization & Quality, 2007, 45(3): 19-21
Authors:MA Xin-guang  ZHANG Yun-fei
Abstract:This paper introduced the practice of Tangsteel's FTSC thin slab continuous casting,and analyzed the cause and mechanism of Tangsteel's FTSC thin slab continuous casting bonding from the molten steel purity and temperature,liquid steel level and oscillation of continuous caster mould,mould taper,equipment,flux and so on,contemporary put forward relevant prevent measures, remarkably reduced bonding rate.
Keywords:thin slab continuous casting  bonding  measure