Abstract:The creep resistance of SP700 (Ti–4.5Al–3V–2Mo–2Fe) is superior to Ti–6–4 (Ti–6Al–4V) at 500 °C under a constant load corresponding to an initial stress of 100 MPa. The β phase grains in the SP700 alloy prefer to orient along the loading axis in contrast to the Ti–6–4 alloy. The grain growth occurs during the stress drop incubation period. The observation of different amounts of negative creep/anelasticity upon loading is closely associated with the difference in the amount of grain/subgrain coarsening.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号