Abstract:Conclusions The growth of pearlite in the process of isothermal transformation of austenite decreases mainly in sections between branches rich in manganese.At 560°C the growth rate of pearlite within branches and between branches is almost identical.With an increase of the manganese concentration from 1.5 to 3.6% the difference in the growth rates of pearlite in branches and between branches increases 7–64 times at 560°C, which is due to the change in the segregation coefficient from 0.82 to 0.56.Institute of Ferrous Metallurgy, Dnepropetrovsk. Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 5, pp. 17–21, May, 1975.