Abstract: | The temperature dependence of acoustic shear velocities are reported for Poly-Penco nylon, type G Plexiglass [poly(methyl methacrylate)], TFE Teflon (tetrafluoroethylene), low- and high-density polyethylene, Lexan (polycarbonate), and Delrin Acetal (nylon). Most of the data were obtained at a frequency of 1 Mc./sec. over the temperature range of 25–100°C. In addition, previously unreported longitudinal velocities to ~125°C. are reported for Lexan and Delrin Acetal. |