Abstract: | Rice husk ash (RHA) obtained from rice mill and hydrated silica from RHA were used as a filler in vulcanized SBR 1502 and the dielectric properties were measured at a frequency of 1592 Hz at room temperature. The optimum hydrated silica content giving a good dielectric constant and conductivity was 125 parts/100 parts rubber and the dielectric loss was also high so that it could be a good insulater. There was no significant change in dielectric constant, dielectric loss and conductivity of SBR 1502 filled with RHA which could be used as high frequency dielectric due to low dielectric loss. |