Abstract: | Conclusions -- The spinning of polyacrylonitrile copolymers into organic baths containing dimethyl sulfoxide and isopropyl alcohol has been investigated. It has been found that the optimum DMSO:IPA ratio in the precipitation bath is 60:40% by wt..-- It has been discovered that the strength of the spun yarn is higher the lower the jet stretch.-- The effect of temperature on orientation stretch ratio has been studied. It has been shown that the optimum temperature for heat stretching of PAN yarn lies in the range 155–160°C.-- The dimethyl sulfoxide content of yarn has been determined by technological transitions. In the final yarn it does not exceed 0.3–1.2% by wt.VNIIPV. Translated from Khimicheskie Volokna, No. 3, pp. 15–16, May–June, 1991. |