首页 | 本学科首页   官方微博 | 高级检索  
     

Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy
引用本文:高飞 王华明. Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy[J]. 中国有色金属学会会刊, 2007, 17(6): 1358-1362. DOI: 10.1016/S1003-6326(07)60277-5
作者姓名:高飞 王华明
作者单位:Laboratory of Laser Materials Processing and Manufacturing, School of Materials Science and Engineering, Beihang University, Beijing 100083, China
摘    要:

关 键 词:TiNi Ti2Ni 磨损 金属合金
收稿时间:2007-07-15
修稿时间:2007-07-15

Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy
Fei GAO,Hua-Ming WANG. Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy[J]. Transactions of Nonferrous Metals Society of China, 2007, 17(6): 1358-1362. DOI: 10.1016/S1003-6326(07)60277-5
Authors:Fei GAO  Hua-Ming WANG
Affiliation:Laboratory of Laser Materials Processing and Manufacturing, School of Materials Science and Engineering, Beihang University, Beijing 100083, China
Abstract:A wear resistant intermetallic alloy consisting of TiNi primary dendrites and Ti2Ni matrix was fabricated by the laser melting deposition manufacturing process. Wear resistance of Ti2Ni/TiNi alloy was evaluated on an abrasive wear tester at room temperature under the different loads. The results show that the intermetallic alloy suffers more abrasive wear attack under low wear test load of 7, 13 and 25 N than high-chromium cast-iron. However, the intermetallic alloy exhibits better wear resistance under wear test load of 49 N. Abrasive wear of the laser melting deposition TiENi/TiNi alloy is governed by micro-cutting and plowing. Pseudoelasticity of TiNi plays an active role in contributing to abrasive wear resistance.
Keywords:TiNi  Ti2Ni  abrasive wear  intermetallic alloy