呋喃树脂砂铸件常见缺陷及防止措施
引用本文:季文华. 呋喃树脂砂铸件常见缺陷及防止措施[J]. 现代铸铁, 2006, 26(5): 76-78
作者姓名:季文华
作者单位:杭州齿轮箱厂,浙江,杭州,311203
摘    要:呋喃树脂砂铸件质量一般比黏土砂铸件好,但如果原材料选择、工艺设计、造型和制芯操作不当。也会产生气孔、粘砂、脉纹、裂纹、夹渣、硬度不足、渗碳、渗硫和球化不良等铸造缺陷。对这些缺陷的产生原因进行了分析,并提出了相应的防止措施。

关 键 词:呋喃树脂砂  缺陷  防止措施
文章编号:1003-8345(2006)05-0076-03
收稿时间:2006-08-15
修稿时间:2006-08-15

Common Defects of Furan Sand Castings and Prevention Measures
JI Wen-hua. Common Defects of Furan Sand Castings and Prevention Measures[J]. Modern Cast Iron, 2006, 26(5): 76-78
Authors:JI Wen-hua
Affiliation:Hangzhou Gear Box Works, Hang zhou 311203, China
Abstract:The quality of furan sand castings is usually better than clay sand castings, however, some defects are also very easy take place with furan sand castings such as blow hole, metal penetration, veining, cracking, slag inclusion, hardness too low, surface recarburation, surface sulphuration, nodularity degeneration etc, which were usually caused by improper raw materials selection, improper method design, incorrect moulding or/and core-making. The defects reasons were analyzed, and correspond prevention measures were suggested.
Keywords:furan resin sand   defect   prevention measures