首页 | 本学科首页   官方微博 | 高级检索  
     

转炉炼钢氧气压力的选择
引用本文:杨文远,王丽丽,肖尊湖,王明林,刘路长. 转炉炼钢氧气压力的选择[J]. 钢铁, 2014, 49(11): 36-41. DOI: 10.13228/j.boyuan.issn0449-749x.20130603
作者姓名:杨文远  王丽丽  肖尊湖  王明林  刘路长
作者单位:1. 钢铁研究总院工艺所, 北京 100081 2. 鞍山热能研究院, 辽宁 鞍山 114000 3. 涟源钢铁集团有限公司炼钢厂, 湖南 娄底 417009 4. 武汉钢铁集团公司, 湖北 武汉 430083
摘    要: 转炉的工作氧压由喷头马赫数决定,使氧射流对熔池的穿透深度[(L)]与熔池深度[(L0)]有一个合适的比例[(L/L0)]。据实际调查,国内有1/3转炉钢厂的工作氧压不合理。根据理论分析和生产实践经验,转炉的工作氧压应比氧气喷头马赫数所对应的滞止压力高5%~15%,可以减少射流在超音速范围内的激波损失,使氧射流对熔池有较大的冲击深度,也可防止因喷孔出口处的负压而使喷孔快速熔损。在氧气喷头设计和制定供氧制度中还需了解氧气管道压力损失[Δp],用实测法所得到的[Δp]值较为可靠。

关 键 词:转炉  射流  激波  氧气压力  马赫数  
收稿时间:2013-11-02

Oxygen Pressure Selection in BOF
YANG Wen-yuan,WANG Li-li,XIAO Zun-hu,WANG Ming-lin,LIU Lu-chang. Oxygen Pressure Selection in BOF[J]. Iron & Steel, 2014, 49(11): 36-41. DOI: 10.13228/j.boyuan.issn0449-749x.20130603
Authors:YANG Wen-yuan  WANG Li-li  XIAO Zun-hu  WANG Ming-lin  LIU Lu-chang
Affiliation:1. Central Iron and Steel Research Institute, Beijing 100081, Chian 2. Anshan Research Institute of Thermo-Energy,Anshan 114000, Liaoning, China 3. Lianyuan Iron and Steel Group Ltd., Loudi 417009, Hunan, China 4. Wuhan Iron and Steel Group Co., Wuhan 430083, Hubei, China
Abstract:Oxygen pressure of work in BOF is decided by nozzle Mach number. Oxygen jet penetration depth of the bath [(L)] and the bath depth [(L0)] has an appropriate ratio [(L/L0)]. About 1/3 steel plant’s working oxygen pressure is unreasonable in China. According to theoretical analysis and practical experience, working oxygen pressure is usually higher (5%~15%) than stagnant pressure according to Mach. Therefore, shockwave losses of flow jet can be reduced, penetration depth of jet is deeper and nozzle rapid melting caused by negative pressure at nozzle outlet can be prevented. Pressure losses [(Δp)] caused by oxygen passing through pipeline should be understand during nozzle designing. Field measurement method is comparatively reliable to get the pressure loss.
Keywords:converter  jet  shockwave  oxygen pressure  mach number
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《钢铁》浏览原始摘要信息
点击此处可从《钢铁》下载全文