Preparation of Ti3SiC2 with Aluminum by Means of Spark Plasma Sintering
引用本文:ZHUJiao-qun MEIBing-chu CHENYan-lin. Preparation of Ti3SiC2 with Aluminum by Means of Spark Plasma Sintering[J]. 武汉理工大学学报(材料科学英文版), 2003, 18(1): 37-40. DOI: 10.1007/BF02835085
作者姓名:ZHUJiao-qun MEIBing-chu CHENYan-lin
作者单位:Wuhan University of Technology 
摘    要:Polycrystalline bulk Ti3SiC2 material with a high purity and density was fabricated by spark plasma sintering from the elemental powder mixture with starting composition of Ti3Si3Si1-xAlxC2 , where x = 0. 05 -0.2. X-ray diffraction patterns and scanning electron microscopy photographs of the fully dense samples show that a proper addition of aluminum promotes the formation, and accelerates the crystal growth rate of Ti3SIC2, conse-quently results in a high purity of the prepared samples. The synthesized Ti3 SiC2 is in plane-shape with a size of about 10- 25μm in the elongated dimension. Solid solution of aluminum decreases the thermal stability of Ti3SiC2, and lowers the temperature of Ti3SiC2 decomposeing to be 1300 ℃ .

关 键 词:Ti3SiC2 钛硅碳化物 火花等离子体烧结 制备 铝 粉末混合物 X射线衍射 扫描电子显微镜
收稿时间:2002-04-30

Preparation of Ti3SiC2 with aluminum by means of spark plasma sintering
Zhu Jiao-qun,Mei Bing-chu,Chen Yan-lin. Preparation of Ti3SiC2 with aluminum by means of spark plasma sintering[J]. Journal of Wuhan University of Technology. Materials Science Edition, 2003, 18(1): 37-40. DOI: 10.1007/BF02835085
Authors:Zhu Jiao-qun  Mei Bing-chu  Chen Yan-lin
Affiliation:(1) State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, 430070 Wuhan, China
Abstract:Polycrystalline bulk Ti3SiC2 material with a high purity and density was fabricated by spark plasma sintering from the elemental powder mixture with starting composition of Ti3Si1−xAlxC2, where x=0.05–0.2. X-ray diffraction patterns and scanning electron microscopy photographs of the fully dense samples show that a proper addition of aluminum promotes the formation, and accelerates the crystal growth rate of Ti3SiC2, conse-quently results in a high purity of the prepared samples. The synthesized Ti3SiC2 is in plane-shape with a size of about 10–25μm in the elongated dimension. Solid solution of aluminum decreases the thermal stability of Ti3SiC2, and lowers the temperature of Ti3SiC2 decomposeing to be 1300°C. Zhu Jiaoqun: Born in 1964 Funded by the National Natural Science Foundation of China(No. 50172037)
Keywords:titanium silicon carbide  spark plasma sintering  preparation