摘    要:为解决甘肃河西地区混凝土构筑物早期收缩开裂问题,以预湿轻骨料作为内养护材料,通过室内模拟河西地区气候条件,研究了预湿轻骨料对混凝土抗压强度、自收缩、干燥收缩以及毛细管负压等性能的影响。结果表明:预湿轻骨料可以有效改善河西地区气候条件下的混凝土收缩开裂问题;但预湿轻骨料会对混凝土强度产生不利影响,应对其掺量加以控制;预湿页岩陶粒的内养护效果要好于预湿粉煤灰陶粒,且页岩陶粒引入水量为内养护水量的70%时,对混凝土内养护效果最佳。

关 键 词:混凝土  预湿轻骨料  河西地区  内养护  开裂

Effect of Pre-Wetted Lightweight Aggregates on the Shrinkage Cracking Behavior of Concrete in Hexi Area of Gansu
HAN Bo,NAN Xue-li,YANG Lan-lan,TANG Wei-bin,LI Rong-yang. Effect of Pre-Wetted Lightweight Aggregates on the Shrinkage Cracking Behavior of Concrete in Hexi Area of Gansu[J]. Bulletin of the Chinese Ceramic Society, 2019, 38(4): 989-995
Authors:HAN Bo  NAN Xue-li  YANG Lan-lan  TANG Wei-bin  LI Rong-yang
Affiliation:(State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals,Lanzhou University of Technology,Lanzhou 730050,China;School of Material Science and Engineering,Lanzhou University of Technology,Lanzhou 730050,China;Gansu Provincial Communications Planning Survey and Design Institute Co.,Ltd.,Lanzhou 730000,China)
Abstract:To solve the problem of early shrinkage cracking of concrete structure in Hexi area of Gansu Province, used pre-wetted lightweight aggregates as internal curing material, simulated the weather conditions in the Hexi area through the laboratory, the effect of pre-wetted lightweight aggregates on the compressive strength, autogenous shrinkage, dry shrinkage and meniscus depression of concrete was studied. Test results show that the pre-wetted lightweight aggregates can effectively improve the shrinkage and cracking of concrete under the climatic conditions in the Hexi area. However, the pre-wetted lightweight aggregates will have an adverse effect on the strength of the concrete, and the amount of pre-wetted lightweight aggregates shall be controlled. The pre-wetted shale haydite has better internal curing effect than the pre-wetted fly ash ceramsite, and the shale haydite introduces 70% of curing water, which has the best curing effect in the concrete.
Keywords:concrete  pre-wetted lightweight aggregate  Hexi area  internal curing  cracking
本文献已被 CNKI 维普 万方数据 等数据库收录!
点击此处可从《硅酸盐通报》浏览原始摘要信息
点击此处可从《硅酸盐通报》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号