端羟基聚环氧氯丙烷酯化反应研究
引用本文:王静刚,李俊贤,王勃.端羟基聚环氧氯丙烷酯化反应研究[J].化学推进剂与高分子材料,2008,6(4).
作者姓名:王静刚  李俊贤  王勃
作者单位:1. 河南科技大学,河南洛阳,471003
2. 黎明化工研究院,河南洛阳,471000
摘    要:通过端羟基聚环氧氯丙烷(PECH)的酯化,合成了端酯基PECH,用FT-IR和NMR进行了结构表征。优化了酯化反应工艺,结果表明:以乙酸酐为酯化剂,酯化剂与羟基物质的量比为1.6;N-甲基咪唑为催化剂,催化剂质量分数为3.6%;1,2-二氯乙烷为溶剂,反应温度为80℃,反应时间为0.5h,则羟基转化率为100%,收率>94.3%。

关 键 词:聚环氧氯丙烷  酯化  增塑剂

Study on Esterification of Hydroxyl-Terminated Polyepichlorohydrin
WANG Jing-gang,LI Jun-xian,WANG Bo.Study on Esterification of Hydroxyl-Terminated Polyepichlorohydrin[J].Chemical Propellants & Polymeric Materials,2008,6(4).
Authors:WANG Jing-gang  LI Jun-xian  WANG Bo
Abstract:Ester-terminated polyepichlorohydrin was synthesized by esterification of hydroxyl-terminated polyepichlorohydrin and the structures were charactered by FT-IR and NMR. The optimal reaction conditions of esterification was investigated. The result shows that the conversion of hydroxyl is 100% and product yield > 94.3% when acetic anhydride is used as esterifying agent, the molar ratio of esterifying agent to hydroxy group is 1.6, N-methyl imidazole is used as esterification catalyst, the mass fraction of the catalyst is 3.6%, 1,2-dichloroethane is used as solvent, reaction temperature is 80℃, reaction time is 0.5h.
Keywords:polyepichlorohydrin  esterification  plasticizer