首页 | 本学科首页   官方微博 | 高级检索  
     

恒刚度轧制改善R0粗轧机的轧制板形
引用本文:罗军. 恒刚度轧制改善R0粗轧机的轧制板形[J]. 柳钢科技, 2008, 0(4)
作者姓名:罗军
作者单位:热轧厂
摘    要:R0粗轧机安装以来由于轧机两侧刚度差异大以及板形差易导致精轧废钢,一直不能正常使用,通过采用改变轧制控制的方式来改善R0粗轧机板形,使其能正常使用。

关 键 词:轧钢  R0粗轧机  恒刚度轧制  板形

Improvement of Rolling Profile Shape of R0 Roughing Mill with Permanent Rigidity Rolling
LUO Jun. Improvement of Rolling Profile Shape of R0 Roughing Mill with Permanent Rigidity Rolling[J]. , 2008, 0(4)
Authors:LUO Jun
Affiliation:LUO Jun (Hot-strip Mill)
Abstract:The big rigidity differences between two sides of mill and profile shape differences produce finishing scraps since installation of R0 Roughing Mill which can not be operated normally. This R0 Roughing Mill can be put into operation normally through adopting the method of changing rolling control to improve its profile shape.
Keywords:Steel Rolling R0 Roughing Mill Permanent Rigidity Rolling Profile Shape  