泡沫铅对VRLA电池性能的影响
引用本文:戴长松,伊廷锋,王殿龙,胡信国.泡沫铅对VRLA电池性能的影响[J].电池,2005,35(3):219-220.
作者姓名:戴长松  伊廷锋  王殿龙  胡信国
作者单位:哈尔滨工业大学应用化学系,黑龙江,哈尔滨,150001
摘    要:以泡沫铜为基体,采用电沉积铅制备泡沫铅板栅,并将其作为阎控密封铅酸电池的负极集流体,组装成负极限容的实验电池.对实验电池进行了充放电性能测试,结果表明:在20h、10 h、5 h和2 h率放电情况下,泡沫铅电池与铸造板栅电池相比,质量比容量分别提高了23%、36%、35%和44%,活性物质利用率分别提高了5.03%、9.86%、8.79%和9.60%.

关 键 词:阀控密封铅酸电池  容量  板栅  泡沫铅
文章编号:1001-1579(2005)03-0219-02
修稿时间:2004年7月1日

Effects of lead foam on the performance of VRLA battery
DAI Chang-song,YI Ting-feng,WANG Dian-long,HU Xin-guo.Effects of lead foam on the performance of VRLA battery[J].Battery Bimonthly,2005,35(3):219-220.
Authors:DAI Chang-song  YI Ting-feng  WANG Dian-long  HU Xin-guo
Abstract:Based on copper foam substrate, lead foam grid was prepared through electroplating lead and used as negative current collector of valve-regulated lead acid (VRLA) batteries to assemble the test battery, whose capacity was determined by negative capacity.Charge-discharge performance tests were taken to the experimental batteries. The results showed that at 20 h, 10 h, 5 h and 2 h rate discharge, the mass specific capacity of lead foam battery increased 23%, 36%, 35% and 44% than that of casting grid battery, the utilization efficiency of active material improved 5.03%, 9.86%, 8.79% and 9.60% than that of casting grid battery.
Keywords:VRLA battery  capacity  grid  lead foam