Abstract: | Textile cotton wastes were irradiated with γ-rays at different doses and solubilized with 10% NaOH solutions. The regenerated products underwent enzymatic hydrolysis and their degradation pattern was compared with that of the cotton celluloses untreated or treated only with γ-rays. The different samples were characterized by measurements of X-ray diffraction, degree of polymerization, moisture regain and water retention. The structural and morphological modifications induced by the pretreatments were correlated with the variations of kinetic parameters, particularly the Vmax/Km ratio, defined as specificity constant. Only the combination of irradiation with dissolution pretreatments gave a considerable increase of hydrolysis reaction effectiveness. |