Curing Characteristics and Mechanical and Morphological Properties of Styrene Butadiene Rubber/Virgin Acrylonitrile-Butadiene Rubber (SBR/vNBR) and Styrene Butadiene Rubber/Recycled Acrylonitrile-Butadiene Rubber (SBR/rNBR) Blends
Authors:N Z Noriman  Azura Rashid
Affiliation:School of Materials and Mineral Resources Engineering, Universiti Sains Malaysia, Seri Ampangan Nibong Tebal, Seberang Perai Selatan , Penang, Malaysia
Abstract:Curing characteristics and mechanical and morphological properties of styrene butadiene rubber/virgin acrylonitrile-butadiene rubber (SBR/vNBR) and styrene butadiene rubber/recycled acrylonitrile-butadiene rubber (SBR/rNBR) were investigated. Results indicated that the curing characteristics, such as scorch time, t2, and cure time, t90, of SBR/vNBR and SBR/rNBR blends decreased with increasing vNBR and rNBR content. At similar blend ratios, particularly up to 15 phr, SBR/rNBR blends exhibited higher t2 and t90 compared with SBR/vNBR blends. Minimum torque (ML) and maximum torque (MH) of SBR/vNBR blends significantly increased with increasing vNBR content. For SBR/rNBR blends, ML increased with increasing rNBR content, but MH exhibited the opposite trend. Tensile strength, elongation at break (Eb), resilience, and fatigue decreased with increasing virgin and recycled NBR content in both blends. Up to 15 phr, the tensile strength, Eb and fatigue life (Kc) of SBR/rNBR blends were higher than in SBR/vNBR blends. The M100 (stress at 100% elongation), hardness, and cross-linking density of both blends also showed an increasing trend with increasing vNBR and rNBR content. The scanning electron microscopy study indicates that rNBR exhibited a weak rNBR-SBR matrix interaction particularly when more than 15 phr of rNBR was used, thus decreasing the mechanical properties of SBR/rNBR blends.
Keywords:Curing characteristics  Mechanical properties  Morphological study  NBR  Recycled NBR  SBR
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号