Towards the understanding of plasma polymer film behaviour in ethanol: A multi-technique investigation
Authors:Laurent Denis  Damien Thiry  Damien Cossement  Pascal Gerbaux  Fabiola Brusciotti  Isabel Van De Keere  Veerle Goossens  Herman Terryn  Michel Hecq  Rony Snyders
Affiliation:1. Laboratory of Plasma-Surface Interaction Chemistry (PSI Chem), Center of Innovation and Research in Materials and Polymers (CIRMAP), Université de Mons, Place du Parc 20, B-7000 Mons, Belgium;2. Materia Nova Research Center, Parc Initialis, Avenue N. Copernic 1, B-7000 Mons, Belgium;3. Laboratoire de Chimie Organique, Centre de Spectrométrie de Masse, Université de Mons, Place du Parc 20, B-7000 Mons, Belgium;4. Research Group Electrochemical and Surface Engineering, Vrije Universiteit Brussel, Pleinlaan 2, B-1050 Brussels, Belgium
Abstract:Plasma polymer films (PPFs) of allylamine are prepared varying the mean power injected in the plasma (Pmean). The PPF behaviour in ethanol is studied through the analysis of the PPF physico-chemistry and the composition of the resulting ethanol solutions. By Visible light Spectroscopic Ellipsometry (VISSE), it is observed that the well-known decrease of the PPF thickness (Δd) upon immersion decreases as a function of Pmean. This behaviour is attributed to an increase of the PPF cross-linking density (χ). By means of time-of-flight secondary ion mass spectrometry (ToF-SIMS) and further statistical processing of the data by principal component analysis (PCA), we propose a method to discriminate the samples according to χ. A significant increase in the PPF oxygen content is also observed after immersion which is ascribed to reaction between ethanol molecules and trapped radicals of the PPF network. On the other hand, taking into account the specificities of the gas chromatography–mass spectrometry (GC–MS) method, the resulting ethanol solutions are demonstrated to be free of chemical species containing a number of carbon atoms ranging from 7 to 40. However, Δd (accounting for PPF restructuring) might come with the dissolution of PPF materials having less than 7 carbon atoms.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号