摘    要:研究矿渣掺碍对于高强高性能混凝土性能的影响。水胶比为0.28,矿渣掺量达40%,可以配制出早期,后期强度无高于不掺矿渣,而水泥用量高达600kg/m^3的纯水泥混凝土的相应强度,这种配合比的混凝土28天强度在87MPa以上;并且流动性好,可以满足泵送需要。

关 键 词:矿渣掺量  高强混凝土  高性能混凝土  耐久性

An experimental study of effect of quantity of blast furnace slap on the strength and durability of high strength concrete and high performance concrete
Leng Faguang,Feng Naiqian.An experimental study of effect of quantity of blast furnace slap on the strength and durability of high strength concrete and high performance concrete[J].China Building Materials Science & Technology,2000(1):14-17,41.
Authors:Leng Faguang  Feng Naiqian
Affiliation:Civil engineering department of Tsinghua university
Abstract:This paper studies the effect of quatity of blast furnace slag on the strength and durability of high strength concrete and high performance concrete. When the w/e is 0.28, and the quantity of blast furnace slag is 40 percent of total binder by weight, the strength of blast-furnace-slag concrete is higher than that of pure Portland cement concrete whose cement content is up to 600kg/m~3. The strength of blast-furnace-slag concrete at 28 day is higher than 87MPa; its workability is good to suit for pumping constrction; it has low permeability and its service life is up to 75 years. The optimization quantity of blast-furnace-slag is about 40 percent at long age and 10 percent at early age.
Keywords:Quantity of Blast-Furnace-Slag High-Strength ConcreteHigh-performance Concrete Diffusion Coefficientof  Chloride Ions Electric Quantity Optimlzation Quantity Pumping Concrete Permeability Service Life