BHW35钢电渣焊后亚温淬火
引用本文:刘颖,崔约贤.BHW35钢电渣焊后亚温淬火[J].热能动力工程,1996,11(2):108-111.
作者姓名:刘颖  崔约贤
作者单位:哈尔滨锅炉有限责任公司,哈尔滨工业大学
摘    要:BHW35钢电渣焊后经正火加严温淬火和回火处理,其焊接接头及母材的冲击韧性大幅度提高,且强度也保持了较高的水平,从而解决了HBW35钢电渣焊缝冲击专访性偏低的问题。

关 键 词:BHW35钢  淬火  冲击韧性  电渣焊  压力容器

Sub-temperature Quench of BHW35 Steel after Electroslag welding
Liu Ying,Xiao Yueling, Chang Fanghua,You Mo.Sub-temperature Quench of BHW35 Steel after Electroslag welding[J].Journal of Engineering for Thermal Energy and Power,1996,11(2):108-111.
Authors:Liu Ying  Xiao Yueling  Chang Fanghua  You Mo
Abstract:The treatment of normalizing, sub-temperature quenching and tempering to W35 steel after electroslag welding can improve the impact toughness of the welding contacts and the mother steel, with the high strength being maitsined. The problem of low impact toughness of electroslag welding seam of BHW steel has been therefor resolved.
Keywords:BHW35 Steel  Welding  Impact Toughness  Quench  